Select Your Region
Golpanol® HD is used as a top brightener in bright and semi-bright nickel electroplating baths at a concentration of 100 – 300 mg/l.
Concentration: 78-82%
Iodine Color: <15
Density: 1.01-1.03 g/cm3
pH: 3.5-6.5
Primary Chemistry:
3-Hexyn-2,5-diol
Conor Robertson, Technical Specialist
Product recommendations backed by technical expertise.
Fast answers to formulation and application questions.
Golpanol® HD is used to formulate brightener additives employed in the electroplating industry and as an inhibitor for anodizing aluminium.
Dull or Hazy Deposits on Electroplated Metal Surface
Strategically located across North America and EMEA for fast, reliable delivery. Every order, every time.
We’ve detected that you are located in a different region than the region selected on the website. Would you like to change your region?
Current Region: English - United States